AWS D1.1/D1.1M:2025 · 条項 5

What Is a 溶接施工要領書 (WPS)?

A 溶接施工法 specification (WPS) is a written document that defines the welding variables required to produce a sound 溶接 for a given application. Under AWS D1.1:2025 Clause 5.2.1, all 事前認定 WPSs shall be prepared by the 施工業者 as written prequalified WPSs. The WPS is the instruction set the 溶接士 follows — it specifies what to weld, how to weld it, and under what conditions.

Per AWS D1.1:2025 Clause 5.2.1: “All prequalified WPSs shall be prepared by the Contractor as written prequalified WPSs.”

The one-sentence version: The WPS is the recipe. The PQR is the proof the recipe works. A 事前認定WPS under D1.1 Clause 5 needs no PQR — the 基準 has already validated it through decades of industry use.

WPS Definition and Purpose

A Welding Procedure Specification is a formal written document that prescribes the variables for a specific welding application to assure repeatability. Every time a qualified welder picks up that WPS, they weld to the same parameters — same process, same 母材群, same 溶加材, same 予熱, same technique 限界値. That consistency is what produces predictable 機械的性質 and code 適合.

Under AWS D1.1:2025 Clause 5.2.1, the written prequalified WPS may follow any convenient format. AWS Annex J provides sample forms, but fabricators can use their own format provided all required variables per 表 5.5 are addressed. The WPS is a living document: changes to essential variables beyond permitted tolerances require a new or revised WPS. For a step-by-step form walkthrough, see our Annex J field ガイド.

The WPS is the starting point for all welded construction under D1.1. Before the first arc is struck, the Contractor must have a 文書WPS that covers the specific combination of 母材, process, filler metal, position, and 継手形状 being used. No WPS, no compliant weld.

What a WPS Must Contain

D1.1:2025 Table 5.5 has two sections. The upper section lists 21 variables that must be included in a written prequalified WPS. The lower section adds 10 variable tolerance entries (items 22–31) defining allowable ranges for parameters like 電流, 電圧, and 溶接速度. Of the 21 required variables, only the 溶接工程 (item 1) carries a footnote requiring a separate WPS when changed — changes to other variables require a revised WPS or requalification per Clause 5.2.1.

(1) Welding ProcessSMAW, SAW, GMAW, FCAW — a separate WPS required if changed
(2) Welding PositionFlat, horizontal, vertical, overhead — per Table 5.5
(3) Base Metal GroupPer Table 5.6 — Group I, II, III, IV, or V
(4) Preheat CategoryPer Table 5.11 — 最小 preheat and interpass temp
(5) Filler Metal ClassificationAWS A5.X classification (SMAW, GMAW, FCAW)
(6) Filler Metal / FluxClassification for SAW 電極/flux combination
(7) Electrode DiameterNominal diameter of the electrode or wire
(8–9) Number & Spacing (SAW)Number of electrodes; spacing and orientation for SAW
(10–11) Amperage & Voltage±10% amperage, ±15% voltage tolerance for SAW/FCAW/GMAW
(12) Mode of Transfer (GMAW)Spray, pulse, globular — not short-circuit (GMAW-S)
(13–14) 電流の種類 & PolarityAC or DC; DCEN or DCEP
(15) Wire Feed SpeedSpecified for SAW, FCAW, GMAW
(16) Travel Speed±25% tolerance for SAW/FCAW/GMAW
(17–18) Shielding GasNominal composition and flow rate; ±50% increase or −25% decrease on flow rate
(19) Weld TypeFillet, CJP, PJP, plug, or slot
(20) 開先溶接 DetailsJoint geometry per applicable prequalified figures (Figure 5.1 for CJP, Figure 5.2 for PJP)
(21) Postweld Heat TreatmentPWHT conditions per Clause 5.9 if applicable

The preheat calculator looks up variable (4) directly from D1.1:2025 Table 5.11. The carbon equivalent calculator supports the alternative preheat method from Annex B, which can reduce required preheat for certain steels. Both values belong on the written WPS.

Prequalified WPS vs. Qualification by Testing

D1.1 provides two distinct paths to a compliant WPS. Understanding the difference determines whether you need to run 手順資格 tests before starting production welding.

Clause 5 — Prequalified Path

Prequalified WPS

Exempt from 資格試験 per Clause 6. The code has validated these combinations through industry experience. No test welds, no PQR required.

Requirements: Approved process (SMAW, SAW, GMAW except GMAW-S, FCAW) + base metal from Table 5.6 + filler metal per Table 5.7 + joint from the applicable prequalified figure (Figure 5.1 for CJP, Figure 5.2 for PJP, Figure 5.3 for fillet welds) + preheat per Table 5.11.

Who uses it: Most 鉄骨製作 shops. A36 or A572 Gr.50 steel, 規格 groove or fillet welds, E7018 or E71T-1 wire — fully prequalifiable.

Clause 6 — Qualification by Testing

Qualified WPS + PQR

Required when any element falls outside Clause 5 limits. A 試験溶接 is produced, specimens extracted and tested, results documented on a PQR.

Common triggers: GMAW short-circuit transfer (GMAW-S), joint geometry not in Figure 5.1, base metal not in Table 5.6, GTAW or ESW processes.

Who uses it: Specialty fabricators, pressure-boundary adjacent work, non-standard joint geometries, higher-強度 steels not in Table 5.6.

Which Base Metals Can Be Used in a Prequalified WPS?

D1.1:2025 Clause 5.3 and Table 5.6 define the approved base metals for prequalified WPSs, organized into five groups by strength level. Only steels listed in Table 5.6 may be used without qualification 試験. Common structural steels across the groups include:

Group I: ASTM A36, A53 Gr.B, A106 Gr.B, A131, A139 Gr.B, A381 Gr.Y35, A500 Gr.B/C, A501 Gr.A, A516 Gr.55/60, A524 Gr.I/II, A573 Gr.58/65, A709 Gr.36, A1008 SS, A1011 SS, A1018 SS, API 5L Gr.B and X42, ABS Gr.A/B/D/E.

Group II: ASTM A36 (all thicknesses), A131, A216, A501 Gr.B, A516 Gr.65/70, A529 Gr.50/55, A537 Class 1, A572 Gr.42/50/55, A588, A595, A606, A618, A633 Gr.A/C/D, A709 Gr.36/50/50W/HPS 50W, A710 Gr.A Class 2, A847, A913 Gr.50, A992, A1066 Gr.50, A1085, API 2H/2MT1/2W/2Y, API 5L X52, ABS.

Group III: ASTM A537 Class 2, A572 Gr.60/65, A633 Gr.E, A710 Gr.A Class 2 and Class 3, A913 Gr.60/65, A1018 HSLAS Gr.60/70, A1066 Gr.60/65.

Group IV: ASTM A709 HPS 70W, A913 Gr.70, A1066 Gr.70.

Group V: ASTM A913 Grade 80 — the highest-strength prequalified base metal in Table 5.6. Note: per Table 5.6 footnote, the 入熱 limitations of Clause 7.7 (which applies to quenched and tempered steels) do not apply to A913 Grades 60, 65, 70, or 80.

For steels not in Table 5.6, Clause 6.2.1 governs qualification by testing. The mill test report (MTR) is the document that confirms your base metal meets the Table 5.6 specification and grade 要求事項 before welding begins.

Prequalified Welding Processes

Per Clause 5.5.1, four processes are eligible for prequalification under D1.1:

SMAW (被覆アーク溶接) — stick electrodes classified per AWS A5.1 or A5.5. 低水素 electrodes (E7018, E8018, etc.) required for Group III and IV steels and when preheat would otherwise be elevated. Table 5.1 governs SMAW prequalified WPS requirements including 最大 電極径 by position.

SAW (サブマージアーク溶接) — single and multiple electrode configurations. Table 5.2 governs SAW prequalified WPS requirements. Preheat and interpass temperatures for parallel or multiple electrode SAW may be established by the alternate method of Clause 5.7.3 when HAZ hardness testing is performed.

GMAW (ガスメタルアーク溶接) — spray, pulse, and グロビュラー転移 only. GMAW-S (short-circuit transfer) is not prequalified and requires Clause 6 qualification. GMAW and FCAW used in prequalified WPSs shall use constant voltage (CV) power supplies per Clause 5.5.4. Table 5.3 governs GMAW solid wire requirements.

FCAW (Flux-Cored アーク溶接) — both gas-shielded (FCAW-G) and self-shielded (FCAW-S) variants. Table 5.4 governs FCAW and GMAW cored wire requirements. シールドガス composition for GMAW and FCAW-G shall conform to AWS A5.32M/A5.32 per Clause 5.6.4.

WPS vs. PQR — The Difference

These two documents are related but serve completely different functions. Confusing them is one of the most common errors in welding documentation.

The WPS is the recipe — it tells the welder what to do. Process, base metal, filler metal, joint geometry, preheat, electrical parameters, technique. It lives on the shop floor and the welder references it during production.

The PQR is the proof the recipe works — it documents that a test weld produced to the WPS parameters passed 機械試験. Tensile, bend, and impact tests (when required) confirm the procedure produces welds with adequate strength, ductility, and toughness. The PQR supports the WPS; the WPS references the PQR.

A prequalified WPS under D1.1 Clause 5 requires no PQR. The code itself serves as the technical justification. This is a major advantage of D1.1 over ASME Section IX, which requires procedure qualification for every WPS with no prequalified exemption.

Postweld 熱処理 (PWHT)

PWHT may be included in a prequalified WPS provided it is approved by the Engineer and the following five conditions of Clause 5.9 are met: (1) the base metal minimum yield strength shall not exceed 50 ksi [345 MPa]; (2) the steel shall not be quenched and tempered (Q&T), quenched and self-tempered (Q&ST), thermo-mechanical controlled process (TMCP), or cold-worked to achieve higher mechanical properties (e.g., certain grades of ASTM A500 tubing); (3) there shall be no notch toughness requirements for the base metal, HAZ, or 溶接金属; (4) adequate strength and ductility data for the weld metal in the PWHT condition shall be available; and (5) PWHT shall be conducted in conformance with Clause 7.8.

For higher-strength steels (Group III and IV) and Q&T steels, PWHT considerations are critical. The heat input calculator helps control the thermal cycle that affects HAZ properties in these materials.

Calculators That Feed Your WPS

The variables that go into a written WPS are not guesses — they come from D1.1 table lookups and calculations. These tools produce the values directly.

"A WPS is the welder's blueprint. Without it, you're making engineering decisions at the arc — and that's not where engineering decisions should be made."

— Standard CWI instruction, reflecting D1.1:2025 Clause 5.2.1 requirements for written WPSs

Frequently Asked Questions

A welding procedure specification (WPS) is a written document that defines all the welding variables required to produce a sound weld for a given application. Under AWS D1.1:2025 Clause 5.2.1, all prequalified WPSs shall be prepared by the Contractor as written documents. The WPS specifies the welding process, base metal, filler metal, joint design, preheat and interpass temperatures, welding position, electrical characteristics, and technique. It is the instruction set the welder follows on the job.

A WPS is the recipe — it tells the welder what to do. A PQR (Procedure Qualification Record) is the proof that the recipe works. When a WPS cannot be prequalified under D1.1 Clause 5, it must be supported by a PQR: a test weld is made to the proposed WPS, specimens are extracted and tested mechanically, and the results are documented on the PQR. The WPS references the PQR as its technical basis. A prequalified WPS under Clause 5 does not require a PQR.

Under AWS D1.1:2025 Clause 5.1, a prequalified WPS is exempt from the qualification testing required in Clause 6. To be prequalified, the WPS must use an approved welding process (SMAW, SAW, GMAW except short-circuit transfer, or FCAW), a base metal listed in Table 5.6, a filler metal per Table 5.7, a joint detail from the applicable prequalified figure (Figure 5.1 for CJP, Figure 5.2 for PJP, Figure 5.3 for fillet welds), and preheat per Table 5.11. All prequalified WPSs must be written documents. Changes to the essential variables listed in Table 5.5 beyond permitted ranges require a new or revised WPS.

Essential variables are the welding parameters that, when changed beyond specified limits, require a new or revised WPS. For prequalified WPSs under D1.1:2025, Table 5.5 lists 21 variables that must be included in a written WPS, including welding process, position, base metal group, preheat category, filler metal classification, electrode diameter, amperage, voltage, travel speed, shielding gas, mode of transfer (GMAW), weld type, and postweld heat treatment. A separate WPS is required when the Welding Process (item 1) is changed — it is the only Table 5.5 variable carrying that specific requirement (footnote a). Changes to other variables beyond permitted tolerance ranges require a new or revised WPS per Clause 5.2.1.

Under D1.1:2025 Clause 5.5.1, the prequalified processes are SMAW, SAW, GMAW (except GMAW-S, short-circuit transfer), and FCAW. GTAW, ESW, EGW, and GMAW-S are code-approved processes but require WPS qualification by testing per Clause 6 and are not eligible for prequalification. GMAW and FCAW used with prequalified WPSs must use constant voltage (CV) power supplies per Clause 5.5.4.

D1.1:2025 Annex K (Informative — not part of the standard) provides a reference checklist of code subclauses that a prequalified WPS must address. It covers provisions across Clauses 1, 4, 5, 7, 9, and 10, including general WPS requirements (5.2–5.8), base metal (5.3), prequalified processes (5.5.1), filler metal matching (5.6.1), preheat (5.7), joint details (5.4.1 CJP, 5.4.2 PJP), essential variables (Table 5.5), and fabrication requirements such as minimum fillet weld sizes (7.13), base metal preparation (7.14), and backing (7.9). Annex J provides sample WPS forms. The WPS may follow any convenient format provided all required variables are addressed.